MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sinotek Materials C Graphite Roll
Categories: Carbon; Graphite

Material Notes: Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and good elasticity. With this as raw material, manufacturer produces reinforced graphite sheet, spiral wound gasket, flexible graphite packing ring, and reinforced graphite gasket.

Information provided by Sinotek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.700 - 1.50 g/cc0.0253 - 0.0542 lb/in³± 0.06
Thickness 150 - 1500 microns5.90 - 59.0 mil<1±0.03 :: 1-1.5±0.05 :: >1.5±0.3
 
Chemical PropertiesMetricEnglishComments
Ionic Impurities - Cl (Chloride) <= 45 ppm<= 45 ppm
 
Mechanical PropertiesMetricEnglishComments
Resilience >= 10>= 10% Recovery/Resilience at density = 1.0 g/cm3
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 99 %99 %
Sulfur, S <= 0.13 %<= 0.13 %
 
Descriptive Properties
Compressibility>40%Density 1.0g/cm3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Graphite, Carbon, C
BACT Metal-Dylyn® Diamond-Like Nanocomposite Coating
BACT Dylyn® Diamond-Like Nanocomposite Coating
BACT DLC Diamond-Like Coating
Aremco Pyro-Paint™ 634-GR High Temperature Refractory Coating, GR >95%

CSINOT65 / 2122

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.