MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Mitsubishi PA-CX12 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: PA-CX12 is a high-performance nylon filament with a broad range of mechanical and chemical properties. These properties include, but are not limited to, high impact (even at low temperatures), crack & scratch resistance, food/water contact acceptable, superior chemical & weathering resistance backed by a very low water absorption and excellent dimensional stability. PA-CX12 is the perfect nylon filament for the (semi) professional print user who is looking for the perfect combination of printability and mechanical properties.

Features:

  • High-performance industrial grade nylon
  • Strong & Flexible
  • High impact, abrasion, crack & scratch resistance
  • Superior chemical & UV resistance
  • Excellent dimensional stability
  • Low water absorption
  • Food Contact Approved
Colors: M-ABS is available from stock in 12 colors. Other colors on request

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/ccISO 1183
Moisture Absorption 6.50 %6.50 %ISO 62
Filament Diameter 1750 µm1750 µmTolerance: 50 µm, =95% Roundness
 2850 µm2850 µmTolerance: 100 µm, =95% Roundness
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 280 °C
15 g/10 min
@Load 4.76 lb,
Temperature 536 °F
ISO 1133
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8181ISO 868
Tensile Strength, Yield 60.0 MPa8700 psiISO 527
Elongation at Break 50 %50 %ISO 527
Elongation at Yield 8.0 %8.0 %ISO 527
Tensile Modulus 1.40 GPa203 ksi(E); ISO 527
Charpy Impact, Notched 1.40 J/cm²6.66 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 240 - 260 °C464 - 500 °FISO 11357
Vicat Softening Point 110 °C230 °FISO 306 B
 
Processing PropertiesMetricEnglishComments
Processing Temperature 250 - 270 °C482 - 518 °FPrinting Temperature
Drying Temperature 110 - 130 °C230 - 266 °F
Dry Time 3.00 hour3.00 hour
 
Descriptive Properties
Bed Temp=100°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMITS9829 / 301054

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.