MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Arlon CLTE-XT High Precision Ceramic PTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.

CLTE-XT is a micro-dispersed ceramic PTFE composite utilizing a woven fiberglass reinforcement to provide the highest degree of stability, critical in multi-layer designs.

  • Ceramic/PTFE microwave composite
  • High thermal conductivity
  • Lowest Insertion Loss in class
  • Loss Tangent (0.0012)
  • Tightest Dielectric constant and Thickness tolerance
  • Electrical phase stability vs. temperature

Benefits:

  • Excellent thermal stability of Dk and Df
  • Phase stability across temperature
  • High degree of Dimensional stability required for complex, multi-layer boards
  • Excellent CTE in X, Y and Z directions

Typical Applications:

  • Defense Microwave/RF Applications
  • Radar Manifolds
  • Phase Fed Array Antennas
  • Microwave Feed Networks
  • CNI (communication, navigation and identification) Applications
  • SIGINT, Satellite and Space Electronics
  • Phase Sensitive Electronic Applications

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: Arlon Materials for Electronics (MED) is a major manufacturer of specialty high performance laminate and prepreg materials for use in a wide variety of printed circuit board (PCB) applications and in several distinctive markets.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.02 g/ccASTM D792 Method A
Water Absorption 0.020 %IPC TM-650 2.6.2.1
Outgassing - Total Mass Loss 0.010 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
Water Vapor Recovered; NASA SP-R-0022A
 0.020 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
NASA SP-R-0022A
Collected Volatile Condensable Material 0.00 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
NASA SP-R-0022A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 3400 psiCross; IPC TM-650 2.4.18.3
 4000 psiMachine; IPC TM-650 2.4.18.3
Modulus of Elasticity 260 ksiIPC TM-650 2.4.18.3
Flexural Strength 9.00 ksiCross; IPC TM-650 2.4.4
 9.50 ksiMachine; IPC TM-650 2.4.4
Compressive Modulus 244 ksiASTM D3410
Poissons Ratio 0.23ASTM D3039
Shear Modulus 0.730 GPaCalculated
Peel Strength 9.00 pliTo Copper (1 oz./35 micron); After Thermal Stress; IPC TM-650 2.4.8
 10.0 pliTo Copper (1 oz./35 micron); After Process Solutions; IPC TM-650 2.4.8
 11.0 pliTo Copper (1 oz./35 micron); At Elevated Temperatures; IPC TM-650 2.4.8.2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.85e+14 ohm-cmE24/125; IPC TM-650 2.5.17.1
 4.25e+14 ohm-cmC96/35/90; IPC TM-650 2.5.17.1
Surface Resistance 5.48e+13 ohmE24/125; IPC TM-650 2.5.17.1
 2.49e+14 ohmC96/35/90; IPC TM-650 2.5.17.1
Dielectric Constant 2.79 - 2.98
@Frequency 1e+10 Hz
varies by thickness; IPC TM-650 2.5.5.5
 2.94
@Frequency 1e+6 Hz
may vary by thickness; IPC TM-650 2.5.5.3
Dielectric Strength 1000 V/milIPC TM-650 2.5.6.2
Dielectric Breakdown 58000 VIPC TM-650 2.5.6
Dissipation Factor 0.0011
@Temperature -40.0 °C
 0.0013
@Temperature 140 °C
 0.0012
@Frequency 1e+6 Hz
IPC TM-650 2.5.5.3
 0.0012
@Frequency 1e+10 Hz
IPC TM-650 2.5.5.5
Arc Resistance 250 secIPC TM-650 2.5.1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.00 µm/m-°C
@Temperature 50.0 - 150 °C
IPC TM-650 2.4.41
CTE, linear, Transverse to Flow 20.0 µm/m-°C
@Temperature 50.0 - 150 °C
z direction; IPC TM-650 2.4.24
Thermal Conductivity 0.560 W/m-KASTM E1461
Decomposition Temperature 501 °CInitial; IPC TM-650 2.4.24.6
 554 °C5 percent; IPC TM-650 2.4.24.6
Flammability, UL94 V-0
 
Descriptive Properties
IPC Delamination - T260 (minutes)> 60IPC TM-650 2.4.24.1
IPC Delamination - T288 (minutes)> 60IPC TM-650 2.4.24.1
IPC Delamination - T300 (minutes)> 60IPC TM-650 2.4.24.1
Temperature Coefficient of Dielectric (ppm/°C)-9IPC TM-650 2.5.5.5
Z-Axis Expansion (%)1.2IPC TM-650 2.4.24 (50-260°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Osprey CE7 Al-Si Controlled Expansion Alloy
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy)
Borosilicate Glass, Low Expansion
MarkeTech AN 180 Aluminum Nitride Ceramic Substrate, 99% Purity
Schott P-SF8 Glass

PARLM9867 / 149020

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.