MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lotte Chemical Titan TITANLENE® LDF268GG Low density polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: LDF268GG is a low density polyethylene resin for film extrusion. LDF268GG has medium slip and anti-block additives. LDF268GG meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 2.1 & (c) 2.2.

Applications:

  • High clarity thin film
  • Food wrap
  • Diaper backing
  • Textile packaging

Additives:

  • Medium slip
  • Antiblock

Advantages:

  • Excellent transparency
  • Good drawdown
  • Excellent process ability

Information provided by Titan Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Base Resin Density 0.922 g/ccASTM D1505
Thickness 30.0 micronsextruded at 2.5:1 BUR
Base Resin Melt Index 5.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 250 %ASTM D882
Film Elongation at Break, TD 440 %ASTM D882
Elmendorf Tear Strength, MD 9.50 g/micronASTM D1922
Elmendorf Tear Strength, TD 4.00 g/micronASTM D1922
Dart Drop 2.50 g/micronASTM D1709
Film Tensile Strength at Break, MD 19.6 MPaASTM D882
Film Tensile Strength at Break, TD 17.7 MPaASTM D882
1% Secant Modulus, MD 31291 psiASTM D882
1% Secant Modulus, TD 35558 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 93.0 °Cresin; ASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 5.0 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 160 - 180 °C
Blow-up Ratio (BUR) 2.5
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem BI 818 LDPE Injection Molding Polyethylene
Chevron Phillips 4538B LDPE Injection Molding Resin
Chevron Phillips KN 230B LDPE Injection Molding Resin
Braskem BC818 Extrusion Coating Low Density Polyethylene
Carmel Olefins Ipethene® 111 Low Density Polyethylene

PTITAN71 / 70437

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.