Titanpro® SM128 has good melt strength and an excellent balance of stiffness and impact properties. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvants meet their respective FDA regulations and 21 CFR 177.1520(b). In summary, this resin meets the FDA criteria covering safe use of polyolefin articles and component of articles intended for food contact use. Applications: - Sheet, thermoforming, pipe, profile extrusion, pipe fitting.
- Automotive parts.
- Blow molded articles.
Advantages: - Excellent balance of properties.
- Excellent low temperature impact resistance.
- Excellent heat stability.
Fabrication: - Equipment - general extrusion or blow/injection molding machines.
- Techniques - standard processing.
Information provided by Titan Chemicals CAS# 9010-79-1 |