MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Polyplastic Compounds Armlen® PP-1FRX Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: A low-combustible polypropylene. Designed for injection molding and injection molding or extrusion of various items and parts for construction, electrical tools, machine engineering, household appliances, transportation and etc. Available in black color.

Information provided by Polyplastic Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0090 - 0.012 cm/cm0.0090 - 0.012 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 - 0.012 cm/cm0.0090 - 0.012 in/inISO 294-4
Melt Flow 1.3 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.3 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5050ISO 868
Elongation at Break 395 %395 %ISO 527-1
Flexural Strength 21.0 MPa3050 psiat maximum load; ISO 178
Flexural Modulus 1.04 GPa151 ksiISO 178
Charpy Impact Unnotched  4.00 J/cm²
@Temperature -50.0 °C
19.0 ft-lb/in²
@Temperature -58.0 °F
ISO 179-1
 4.70 J/cm²
@Temperature 23.0 °C
22.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 550 V550 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 °C320 °FISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FISO 75
Flammability, UL94 V-0V-0
Glow Wire Ignition Temperature 960 °C1760 °FIEC 60695-2-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 °C464 °F
Mold Temperature 60.0 °C140 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLPLC036 / 307108

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.