MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Lucas-Milhaupt Silvaloy® A56T Flux Coated Rod Brazing Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Silvaloy A56T Flux Coated Rod has the lowest brazing temperature, best wetting, and best flow of all the cadmium free alloys. It has a slight plastic range which may be noticed during melting on some applications. Its low zinc content minimizes problems due to longer heating cycles or due to excessive heating. It is often selected for use on silver or stainless steel due to its excellent color match. Typical applications are the joining of ferrous, non-ferrous, and dissimilar metals and alloys with close joint clearances.

Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).

Key Words: AWS BAg-7
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 9.49 g/cc9.49 g/cc
Density 9.492 g/cc0.3429 lb/in³
Water Absorption 15 - 35 %15 - 35 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000145 ohm-cm0.0000145 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Melting Point 618.3 - 651.7 °C1145 - 1205 °F
Solidus 618.3 °C1145 °F
Liquidus 651.7 °C1205 °F
Maximum Service Temperature, Air 204 °C400 °Fcontinuous
 316 °C600 °Fintermittent
 
Processing PropertiesMetricEnglishComments
Processing Temperature 651.7 - 760 °C1205 - 1400 °FBrazing Temperature
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 21 - 23 %21 - 23 %
Other, total <= 0.15 %<= 0.15 %
Silver, Ag 55 - 57 %55 - 57 %
Tin, Sn 4.5 - 5.5 %4.5 - 5.5 %
Zinc, Zn 15 - 19 %15 - 19 %
 
Descriptive Properties
Boric Acid %25-40percentage of flux
ColorWhite
Electrical Conductivity (% IACS)11.9
Potassium Bifluoride %10-30.0percentage of flux
Potassium Fluoride %5-15.0percentage of flux
Potassium Fluoroborate %5-20.0percentage of flux
Potassium Tetraborate %15-25percentage of flux

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucas-Milhaupt Silvaloy® A56T Brazing Alloy
Lucas-Milhaupt Silvaloy® 501 Brazing Alloy
Lucas-Milhaupt Silvaloy® 50 Brazing Alloy
Materion Silseal® 650 Silver-Copper Brazing Alloy
Lucas-Milhaupt Silvacore® A50N Flux Cored Brazing Alloy

NBRW044 / 79820

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.