MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro DESMODURE® N 3900 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Low-viscosity, aliphatic polyisocyanate resin based on hexamethylene diisocyanate. As the hardener for weather-stable coating systems.

Properties / Applications: Desmodur® N 3900 is used to formulate high-solids systems for automotive refinishing, transportation coating and plastics coating.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccDIN EN ISO 2811
Viscosity 630 - 830 cPDIN EN ISO 3219/A.3
 
Thermal PropertiesOriginal ValueComments
Flash Point 203 °CDIN 22 719
 
Descriptive Properties
Color<40Hazen, M017-EN 1557
Content<0.25%Monomeric HDI, M106-IOS 10283
 23-24%NCO, M105--ISO 11909

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro DESMODURE® PL 340 BA/SN Polyurethane
Covestro DESMODURE® N 3800 Polyurethane
Covestro DESMODURE® N 3790 BA Polyurethane
Covestro DESMODURE® N 3600 Polyurethane
Covestro DESMODURE® N 3400 Polyurethane

PCOVEST0564 / 202347

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.