MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BYK Claytone® TP Rheological Additive
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Claytone TP is a modified montmorillonite designed for use in aliphatic systems containing aromatic solvent or aromatic-aliphatic solvent blends that display low to medium polarity. Claytone TP demonstrates high gelling efficiency, reproducible viscosity and thixotropic development, a high degree of sag control and prevents hard settling of pigments and fillers. Claytone TP has proven to be a reliable and reproducible rheological additive for use in oil based traffic paints.

Applications:

  • Oil based traffic paint

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 37.0 lb/ft³
Density 1.70 g/cc
Particle Mesh Size 200 Mesh98%
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 2.0 %
Loss on Ignition(%) 38.5 %
@Temperature 1000 °C
 
Descriptive Properties
Color/FormVery light cream, finely divided powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK Claytone® TG Rheological Additive for the Oilfield
BYK Claytone® IMG 400 Gellant for Oil Mud Systems
BYK Claytone® II Organophilic Bentonite
BYK Claytone® HY Rheological Additive
BYK Claytone® HT Rheological Additive

PBYK029 / 185026

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.