VESTAMID® DX9330 NC is a PA 612 base polymer without any stabilizers and other additives. VESTAMID® DX9330 NC is suitable for both extrusion as well as injection molding. Usually VESTAMID® DX9330 NC is only used in special cases when additives are not preferable, or processing aids are not necessary, e.g. filament extrusion. Based on the perfect balance of amino and carboxyl end groups this material is easy to process and to dye. The typical characteristics of PA 612 are moderate water absorption, good dimensional stability and almost unchanged properties at varying ambient humidity. VESTAMID® DX9330 NC is supplied as cylindrical granules, ready for processing, in moisture-proof bags. The processing temperature should be within a range of 250°C to 290°C. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C. Dry properties listed below Industrial Sector: Sustainable, Sports and Lifestyle Sustainability: Sustainable electricity Processing: Injection molding Delivery form: Pellets, Granules Conformity: Food contact Additives: Unfilled Applications: Medium viscosity Color: Natural colorInformation provided by Evonik. |