MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Zircar Zirconia ZR-RIG Zirconia Rigidizer
Categories: Ceramic; Machinable Ceramic; Oxide; Zirconium Oxide

Material Notes: Zircar Zirconia Rigidizer Type ZR-RIG is formulated for the surface hardening of all Zircar zirconia fiber products and for use in the fabrication of zirconia composites from Zircar zirconia textiles. Such composites are comprised of a matrix of zirconia fibers reinforced with sub-micron zirconia particles. Type ZR-RIG has the same fired composition as Zircar zirconia fibers and forms a fully stabilized zirconia body upon curing.

ZR- RIG contains sub-micron particles of yttria-stabilized zirconia suspended in a zirconium acetate aqueous solution. The water based rigidizer, as supplied, has the consistency of a light house paint. Should the rigidizer become too thick during use for complete penetration into the surface of the zirconia fiber product, the rigidizer can be thinned by small additions of de-ionized or distilled water.

Features:

  • High Purity
  • High Temperature Stability to 2200°C
  • Withstands Water and Steam after curing
  • Safe to Use – Non-Flammable
  • Available in Two Sizes; Pint or Quart
  • Available ‘Off the Shelf’

Information provided by Zircar Zirconia.

Key Words: ZrO2, zirconium oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.87 g/cc
Solids Content 53 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 2590 °C
 
Component Elements PropertiesOriginal ValueComments
HfO2 1.0 - 2.0 %
Y2O3 10 %
ZrO2 88 - 89 %
 
Descriptive Properties
Trace Inorganics<0.3%
Weight Per Pint885 grams

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aremco Pyro-Paint™ 634-ALP High Temperature Refractory Coating
Aremco Ceramacast™ 646 Castable Ceramic
Anderman Ceramics EZZ 66P Zircon
Anderman Ceramics EZM 96 Zirconia, 96.5%, Magnesia-Stabilized
DuPont Silastic® C7-4550 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer

C6ZIR007 / 2763

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.