MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Permabond UV7141 UV-curable Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Permabond UV7141 is a UV-curable adhesive with a secondary anaerobic cure mechanism. This makes it ideal for bonding materials such as ceramic-coated glass, mirrors, etc. where UV-light cannot penetrate to provide full cure in shadow areas. This dual cure mechanism helps speed up production rates. The UV cure tacks the components in place in seconds, reducing the need for jigging. The bulk of the adhesive then cures more slowly to produce optimum performance.

Features & Benefits:

  • Cures in shadow areas
  • High shear strength
  • Excellent environmental resistance
  • 100% solids, no solvents
  • Excellent adhesion to metal and glass

Information provided by Permabond.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccUncured
Viscosity 1000 - 2000 cP
@Temperature 25.0 °C
Uncured
Storage Temperature 5.00 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60 - 70
Tensile Strength 20.0 MPaASTM D2095
Elongation at Break 20 - 50 %
Adhesive Bond Strength 14.0 - 17.0 MPaGlass/steel, Shear
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.0
@Frequency 1e+6 Hz,
Temperature 25.0 °C
Dielectric Strength 10.0 - 12.0 kV/mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 85.0 µm/m-°C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49
UV Transmittance >= 98 %
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 - 1.00 hourAnaerobic cure speed
 3.00 - 6.00 hourAnaerobic working strength
 5.00 - 20.0 secfixture time, (low power 4mW lamp)
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceColorlessUncured
Cure Wavelength (nm)365
Maximum Gap Fill (mm)0.3
Strength Retention10% at 200°CRelative to 0°C
 100% at 0°CRelative to 0°C
 30% at 150°CRelative to 0°C
 75% at 100°CRelative to 0°C
 95% at 50°CRelative to 0°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Resinlab® EP1310 Medium Reactivity Epoxy Encapsulant
Resin Technology Group UV-422 Flexible, UV Curing Sealant
Henkel Loctite® 3872 1 component acrylic/urethane UV/Heat Cure Flexible Adhesive
Henkel Loctite® 3151 1 component acrylic UV/Heat Cure Acrylic Adhesive

PPERMA933 / 162793

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.