MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ITW Chockfast® PHILLYCLAD 1775/620TS Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: PHILLYCLAD 1775/620TS is an excellent general purpose, nontoxic laminating resin system for FRP application requiring rapid and thorough wet out. Excellent for use as a thin laminate protective coating over steel or wood and fabrication of molded fiberglass structures or components.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/cc
Viscosity 1800 - 2000 cP
@Temperature 22.2 °C
1800 - 2000 cP
@Temperature 72.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 27.9 MPa4050 psiASTM D638
Elongation at Break 30 %30 %ASTM D638
Flexural Strength 35.9 MPa5200 psiASTM D790
Flexural Modulus 0.793 GPa115 ksi
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min
@Temperature 22.0 °C
24.0 hour
@Temperature 71.6 °F
Pot Life 40.0 min
@Temperature 22.2 °C
40.0 min
@Temperature 72.0 °F
1 gallon batch
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
ColorClear Amber
Mix Ratio by volume4 to 3
Mix Ratio by weight4.67 to 3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWC9040 / 239550

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.