MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay Engineered Polymers Dexflex® 1001 TPO  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Data provided by Solvay Engineered Polymers.

A thermoplastic olefinic elastomer (TPO) designed for mold-in-color and uncoated automotive airbag covers. This material provides excellent rigidity, durability, and low-temperature toughness; and it is designed to meet automotive interior gloss requirements (2-3 @ 60°). This material is available with integral color in a selected range of earthtones (shades of black, gray and tan).

Uses: Mold-in-color (uncoated) passenger-side airbag covers, incorporating adequate surface texture, and operating in temperature ranges of -40°C to 104°C.

LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.

Key Words: Thermoplastic Olefinic Elastomer; Polyolefin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/ccASTM D792
Linear Mold Shrinkage 0.010 cm/cmASTM D955
Melt Flow 5.3 g/10 minASTM D1238L
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 40ASTM D2240
Tensile Strength, Ultimate 13.0 MPaIV, 2 in/min; ASTM D638
Elongation at Break 23 %ASTM D638
Flexural Modulus 0.400 GPaI.B., TAN, 0.5 in/min; ASTM D790
Izod Impact, Notched NBLow Temp; ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 20.0 °C
Modified; ASTM D696

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Vistamaxx™ 3980FL Propylene-based Elastomer - High Purity, Low Gel
Teknor Apex Monprene® MP-1301A Thermoplastic Elastomer
Radici Heraflex® P 40D 11 I HF 1530 Modified Polypropylene
Multibase Multi-Flex® A 9402 MR TPE Thermoplastic Elastomer
ExxonMobil EXACT™ 3035 Plastomer for Polymer Modification

PSOLC8 / 67992

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.