MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ganpati Exim HA-102 Titanium Dioxide
Categories: Other Engineering Material

Material Notes: HA-102 is anatase type titanium dioxide laminate organic compounds and it is soluble well in solvents of plastics. The product can disperse uniformly and its dispersion time is short. It has small oil absorption, high achromic power and good whiteness. It is a kind of special type titanium dioxide aiming at master batch and plastics developed by our company. It is especially suitable for master batch, plastics and it is also widely used in other professions.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles >= 0.50 %
@Load 0.100 kg,
Temperature 105 °C
>= 0.50 %
@Load 0.221 lb,
Temperature 221 °F
Oil Absorption >= 22.0 %>= 22.0 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 2200 ohm-cm>= 2200 ohm-cm
 
Component Elements PropertiesMetricEnglishComments
TiO2 >= 98 %>= 98 %
 
Descriptive Properties
Solubility>0.5Water Soluble Object
Tint Reducing Power>100compared with standard sample
Value of Aqueous Suspension6.5-8.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGANPATI129 / 317413

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.