MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Hiflex CA 7600 A Thermoplastic Olefinic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Hiflex CA 7600 A is a reactor soft thermoplastic polyolefin (TPO) , manufactured using the LyondellBasell proprietary Catalloy process technology and is stabilized with a standard additive package. The grade is available in natural colored pellet form. Hiflex CA 7600 A is designed for use in injection molding or extrusion compounds when high processability, optimum mechanical and dimensional stability, are key properties. Thanks to its tailored elastomeric phase, Hiflex CA 7600 A features high softness and high toughness at very low temperature and provide high thermal characteristics. Hiflex CA 7600 A is used as a blending partner to improve the overall performances of esthetical interior and exterior automotive parts. Hiflex CA 7600 A provides high filler loading capability and is highly compatible with a wide range of polyolefins and soft plastics. This grade can be either blended or co-extruded with other materials to provide the required property balance. Applications: Exterior Automotive Applications, Impact Modification.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.880 g/ccMethod A; ISO 1183-1
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 26ISO 868
Tensile Strength at Break 11.0 MPaISO 527-1,-2
Elongation at Break 600 %ISO 527-1,-2
Flexural Modulus 180 MPaISO 178
Charpy Impact, Notched 110 kJ/m²
@Temperature -40.0 °C
ISO 179
 NB
@Temperature 23.0 °C
ISO 179
 NB
@Temperature -20.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 163 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 45.0 °Cunannealed; ISO 75B-1,-2
Vicat Softening Point 58.0 °CA50; ISO 306
 
Descriptive Properties
Processing MethodCompounding, Injection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQT7584 / 219221

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.