MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eastman Eastar™ Renew GN001-50 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastar(TM) Renew GN001-50 copolyester is a clear, amorphous material. Because of its clarity, toughness and good melt strength at processing temperatures, it is useful in a variety of processing techniques. Eastar(TM) Renew GN001-50 copolyester may be colored using color concentrates, dry colors or liquid colorants. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED. The GREENGUARD INDOOR AIR QUALITY CERTIFIED mark is a registered certification mark used under license through the GREENGUARD Environmental Institute (GEI). GEI is an industry-independent, non-profit organization that oversees the GREENGUARD Certification Program. The GREENGUARD Certification Program is an industry independent, third-party testing program for low-emitting products and materials for indoor environments. For more information about GEI and to obtain printable certificates for Eastman™ Copolyesters, visit www.greenguard.org Choose Eastman Chemical Company under the Manufacturer category and click search to display a list of our products. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Applications

  • Building materials
  • Closures-fragrance pkg
  • Color cosmetics packaging
  • Compounders
  • Condiments/dressings/sauces packaging
  • Consumer housewares-nfc
  • Fragrance packaging
  • Jams/fruit sauces packaging
  • Large appliances non-food contact
  • Multi-layer film food contact
  • Multi-layer film non food contact
  • Packaging component films
  • Packaging components non food contact
  • Personal care & cosmetics packaging
  • Personal care bottles
  • Personal care packaging
  • Profiles
  • Protective & performance film
  • Shrink film food contact
  • Shrink film non food contact
  • Small appliances non-food contact
  • Strapping
  • Tools
  • Water/sport bottles
Key Attributes
  • Easy primary & secondary operations
  • Excellent clarity
  • Excellent toughness
  • Gamma, ebeam, ETO sterilization stable

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.00200 - 0.00500 cm/cm0.00200 - 0.00500 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 106106ASTM D785
Tensile Strength at Break 28.0 MPa4060 psiASTM D638
Tensile Strength, Yield 50.0 MPa7250 psiASTM D638
Elongation at Break 130 %130 %ASTM D638
Flexural Yield Strength 70.0 MPa10200 psiASTM D790
Flexural Modulus 2.10 GPa305 ksiASTM D790
Izod Impact, Notched  0.370 J/cm
@Temperature -40.0 °C
0.693 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 1.01 J/cm
@Temperature 23.0 °C
1.89 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D4812
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D4812
Puncture Energy  33.0 J
@Temperature 23.0 °C
24.3 ft-lb
@Temperature 73.4 °F
@ Max. Load; ASTM D3763
 50.0 J
@Temperature -40.0 °C
36.9 ft-lb
@Temperature -40.0 °F
@ Max. Load; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C147 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 249 - 271 °C480 - 520 °F
Mold Temperature 16.0 - 38.0 °C60.8 - 100 °F
Drying Temperature 71.0 °C160 °F
Dry Time 6.00 hour6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM4127 / 323750

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.