MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt SILVALOY® 202 (BRAZE™ 202, SILVALOY® A20) Copper Silver Zinc Braze Alloy
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes: Silvaloy 202 is a useful intermediate temperature, low cost brazing alloy for joining a variety of ferrous and nonferrous alloys. It provides a good color match on yellow brasses. Silvaloy 202 is preferred for brazing steel where heat-treating will be combined with brazing in a single operation. Silvaloy 202 is a braze filler metal with rather long melting range. It has a tendency to liquate (i.e. separate into low and high melting constituents) when heated slowly through its melting range. Therefore, it is preferable to use this alloy where the assemblies can be heated rapidly through solidus-liquidus range. Handy Flux or Handy Flux Type B-1 can be used with Silvaloy 202.

Available forms: Wire, strip, engineered preforms, specialty preforms, powder and paste.

Information provided by Lucas-Milhaupt.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 8.45 g/cc
Density 0.305 lb/in³
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000736 ohm-cm23.5% IACS
 
Thermal PropertiesOriginal ValueComments
Melting Point 1315 - 1500 °F
Solidus 1315 °F
Liquidus 1500 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1500 - 1600 °FBrazing Range
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 44 - 46 %
Other, total <= 0.15 %
Silver, Ag 19 - 21 %
Zinc, Zn 34 - 36 %
 
Descriptive Properties
ColorBrass Yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NLUCM9839 / 254784

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.