MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Adstif HA 716J Polypropylene
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Adstif is a trade name for select polypropylene resins with high crystallinity used to produce customer applications, such as thermoformed containers, injection molded packaging and consumer goods. Adstif's property and performance characteristics include high crystallinity, broad processing window, high stiffness and good dimensional stability.

Polypropylene grade HA716J is a high stiffness homopolymer with a broad molecular weight distribution and is specially designed for metalized biaxial oriented films (BOPP) film applications. HA716J offers better hot fill performance and improved metallically barrier levels. HA716J can also be used in lamination film and compounding applications. Applications: Food Packaging Film, Lamination Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccMethod D; ISO 1183-1
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 76ISO 868
Tensile Strength, Yield 36.0 MPaISO 527-1,-2
Flexural Modulus 1800 MPaISO 178
Izod Impact, Notched (ISO) 4.50 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °Cunannealed; ISO 75B-1,-2
Vicat Softening Point 158 °CISO 306
 
Descriptive Properties
Processing MethodBOPP, Compounding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polyram RamOfin RPPC711 Polypropylene, UV Stabilized
Birch Plastics RPP1215 Recycled Polypropylene
Braskem H 504 XP Bioriented Film Polypropylene
Buckeye Polymers BP RPPC 1813 C BLK Polypropylene, Calcium Filled
Buckeye Polymers BP RPPC 2010 CW Polypropylene, Calcium Filled

PEQT7022 / 218661

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.