MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Thermal Ceramics FireMaster Bulk
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: FireMaster Bulk is used in UL Systems CAJ1053 and CAJ3032 for pipe and cable bundle penetrations. These UL systems have been tested to ASTM E814/UL1479. The bulk is a high-temperature fiber which is classified by Underwriters Laboratories (UL) under “Loose Fill Materials (BPHX)” in the UL Building Materials Directory, No. R9464. FireMaster Bulk is used as a fireproof fill, void, or cavity material for several UL systems. It is the base fiber for FireMaster products.

Features:

  • UL-classified, noncombustible material
  • Lightweight/flexible
  • Optional foil facing or encapsulation
  • Low thermal conductivity
  • Resists chemical attack
  • Unaffected by oil or water
  • Completely inorganic
  • Excellent acoustical properties
  • Applications:

  • Fill, void, or cavity material in through-penetration seals (firestops)
  • Seal duct, cable bundle, conduit, tubing, and cable tray penetrations
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Thermal PropertiesOriginal ValueComments
    Melting Point 3200 °F
    Maximum Service Temperature, Air 2300 °F
    Flammability Test 0.00Flame Spread
     0.00Smoke Developed
     0.00Fuel Contributed
     
    Component Elements PropertiesOriginal ValueComments
    Al2O3 45 %
    Other 2.0 %
    SiO2 53 %
     
    Descriptive Properties
    Water Leachable Elements on Surface of Fiber, PPMBoron, 100
     Chlorine, 5
     Fluorine, <5
     Sulfur, 10

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    CTHERM109 / 2429

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.