MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BASF Elastollan® M95A55 Polyester Type Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding applications. Cycle time improvements of up to 25% over standard polyester grade urethanes can be obtained with M-series grades. They exhibit excellent abrasion resistance, toughness, and resistance to fuels.

As with all TPU products this grade must be dried prior to processing.

Property values below are typical values based on molded plaques cured 20 hours at 100°C before testing. Information provided by BASF Corporation.

Key Words: TPU Rubbers
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595ASTM D2240
Tensile Strength, Ultimate 34.5 MPa5000 psiASTM D412
Tensile Stress at Strain  21.0 MPa
@Strain 100 %
3050 psi
@Strain 100 %
ASTM D-412
 30.0 MPa
@Strain 300 %
4350 psi
@Strain 300 %
ASTM D-412
Elongation at Break 410 %410 %ASTM D412
Tear Strength 160 kN/m913 pliASTM D624
Taber Abrasion, mg/1000 Cycles 3535H-18 wheel; ASTM D-1044.
 
Processing PropertiesMetricEnglishComments
Drying Temperature 80.0 - 90.0 °C176 - 194 °FMust be dried. Typical condition.
Dry Time 2 - 4 hour2 - 4 hour
Moisture Content <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Elastollan® 1174D Polyether Type Polyurethane Elastomer
Alliance Polymers Zythane™ 5080A Thermoplastic Polyurethane Elastomer
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
BASF Elastollan® 1154D Polyether Type Polyurethane Elastomer
Austin Novel Materials Texalan® 598A Polyether-based TPU

PSF977 / 67193

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.