MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Albis Plastics GPPS 04A02CL Crystal Unreinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Transparent Grade

Material Notes: Amorphous General Purpose Polystyrene (GPPS)

Characteristics: FDA Compliant: Crystal Clear, High Molecular Weight, Low Melt Flow

Applications: Egg Cartons, Hot or Cold Food Service, Oriented Polystyrene Sheet

Processing: Injection Molding (Melt Temperature: 340-540°F, Mold Temperature: 40-175°F)

Data supplied by Albis Plastics Corporation.

Former ALBIS Plastics product lines have been spun off under the MOCOM brand. This specific grade was discontinued prior to the spin off.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 1.6 g/10 min
@Load 5.00 kg,
Temperature 200 °C
1.6 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 52.4 MPa7600 psiASTM D638
Modulus of Elasticity 2.76 GPa400 ksiASTM D638
Flexural Yield Strength 100 MPa14500 psiASTM D790
Flexural Modulus 3.24 GPa470 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C208 °FASTM D648
Vicat Softening Point 107 °C225 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 171 - 282 °C340 - 540 °FInjection
Mold Temperature 4.00 - 79.0 °C39.2 - 174 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos Nova 3601 General Purpose Crystal Polystyrene
INEOS Styrolution PS 116 N/L GPPS
LG Chemical MI-750 MIPS
Ineos Nova 3504 General Purpose Crystal Polystyrene
Ineos Nova 3100 General Purpose Crystal Polystyrene

PZA1C04 / 21799

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.