MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Covestro Bayblend® FR3021 GR PC/ABS Blend, 15/30% Mineral/Post Consumer recycled Reinforced
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: (PC+ABS)-Blend; 15 % mineral filled; with 30 % post consumer recycled - water bottle content; flame retardant; Vicat/B 120 temperature = 97 °C; increased stiffness; tensile modulus = 4600 MPa; UL recognition 94 V-0 at 1.5 mm

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ISO 1183-1
Viscosity 211000 cP
@Temperature 260 °C
211000 cP
@Temperature 500 °F
Melt; b.o. ISO 11443-A
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/inparallel/normal; b. o. ISO 2577
Melt Flow 11.61 g/10 min
@Load 5.00 kg,
Temperature 240 °C
11.61 g/10 min
@Load 11.0 lb,
Temperature 464 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 41.0 MPa5950 psi50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 66.0 MPa9570 psi50 mm/min; ISO 527-1,-2
Elongation at Break 4.0 %4.0 %50 mm/min; ISO 527-1,-2
Elongation at Yield 2.9 %2.9 %50 mm/min; ISO 527-1,-2
Tensile Modulus 4.60 GPa667 ksi1 mm/min; ISO 527-1,-2
Izod Impact, Notched (ISO) 7.00 kJ/m²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 180-A
Izod Impact, Unnotched (ISO) 70.0 kJ/m²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
ISO 180-U
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C198 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C183 °FISO 75-1,-2
Vicat Softening Point 97.0 °C
@Load 5.10 kg
207 °F
@Load 11.2 lb
120°C/h; ISO 306
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 °C464 °FInjection; ISO 294
Mold Temperature 80.0 °C176 °FInjection; ISO 294
Injection Velocity 240 mm/sec9.45 in/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese SO.F.TER Reblend® 5510M4 20% Mineral-filled PC/ABS alloy
Covestro Bayblend® FR 3021 Polycarbonate + ABS, Mineral Filled
Mitsubishi Iupilon® MB 1700 PC/ABS
Cossa Polimeri ESTABLEND PA 6000 ABS / Nylon 6 Blend
CoorsTek Porcelain

PCOVEST0048 / 201831

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.