Eastman Tritan™ Renew TX1001-50 is an amorphous copolyester with excellent appearance and clarity. Tritan™ Renew TX1001-50 contains a mold release derived from vegetable based sources. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistance. This new-generation copolyester can also be molded into various applications without incorporating high levels of residual stress. Combined with Tritan's outstanding chemical resistance and hydrolytic stability, these features give molded products enhanced durability in the dishwasher environment, which can expose products to high heat, humidity and aggressive cleaning detergents. Tritan Renew TX1001-50 may be used in repeated use food contact articles under United States Food and Drug Administration (FDA) regulations. Tritan™ Renew TX1001-50 is certified to NSF/ANSI Standard 51 for Food Equipment Materials. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation. Applications - Appliances (food contact)
- Chocolate molds
- Compounders
- Consumer electronics
- Consumer housewares - food contact (fc)
- Consumer housewares-nfc
- Displays/in-store fixtures
- Electronic packaging
- Equipment & machinery
- Filtration
- Industrial
- Large appliances non-food contact
- Lighting
- Non-kitchen appliances
- Non-medical housings & hardware for electrical
- Outdoor signs
- Packaging components non food contact
- Packaging tape
- Personal care & cosmetics packaging
- Personal care bottles
- Personal care packaging
- Point-of-purchase
- Protective & performance film
- Small appliances non-food contact
- Sporting equipment
- Tools
- Toys
- Water/sport bottles
Key Attributes- Ease of processing
- Excellent clarity
- Excellent hydrolytic stability
- Fast drying times
- Good chemical resistance
- Good heat resistance
- Outstanding impact resistance
- Quick cycle times