MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Epoxies, Etc 20-3060 Potting And Encapsulating Epoxy Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: 20-3060 is a general purpose, low viscosity epoxy potting and encapsulating resin system. This is a 100% solids system. It therefore does not contain any solvents. 20-3060 is a filled system resulting in excellent dimensional stability and extremely low shrinkage. 20-3060 is characterized by exceptional resistance to impact, vibration, and thermal shock. In addition, this versatile resin system is machinable and ideal for use with meter mix dispensing equipment. Due to its high purity, 20-3060 offers the ultimate in physical, thermal and electrical insulation properties. The cured polymer exhibits excellent resistance to chemicals, moisture, solvents and environmental exposure. 20-3060 is recommended for applications requiring the optimum in over-all properties and where rigid or flexible wire leads protrude directly from the encapsulant. This system eliminates microscopic cracking when leads are flexed. It also adheres extremely well to lead materials, such as vinyl, neoprene, natural rubber, etc... 20-3060 has found wide acceptance as an encapsulant for applications such as transformers, coils, chokes, solenoids, resistors, modules, microcircuitry, resistors, capacitors, etc... 20-3060 has been formulated for ease in handling and its low viscosity aids in pouring, filling voids and air pockets. In addition, the fillers in 20-3060 have been dispersed to minimize any heavy settling.

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/cc
Viscosity 10000 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82
Tensile Strength 10000 psi
Compressive Strength 22500 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.99e+14 ohm-cm
Dielectric Constant 4.51
@Frequency 100 Hz
Dielectric Strength 460 V/mil
Dissipation Factor 0.010
@Frequency 100 Hz
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.430 W/m-K
Maximum Service Temperature, Air 135 °C
Minimum Service Temperature, Air -50.0 °C
Shrinkage 0.50 %
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 3.00 hour
@Temperature 100 °C
 3.00 - 4.00 hour
@Temperature 85.0 °C
Pot Life 78.0 min
@Load 0.200 kg
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFEPOX030 / 316707

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.