MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Pro-fax PH350 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Pro-fax PH350 general-purpose polypropylene homopolymer is available in spherical particle form. This resin has very minimal stabilization, which allows wide design latitude in compounding applications. Additional stabilization is required to protect the resin during melt processing and throughout its useful life. Any additives compounded into this resin will require a re-assessment of its FDA status. Applications: Color Concentrates, Polymer Modifier, Wood Composites

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 33.0 MPa4790 psi50mm/min; ASTM D638
Elongation at Yield 12 %12 %ASTM D638
Flexural Modulus, 1% Secant 1380 MPa200000 psi1.3 in/min, Procedure A; ASTM D790
Izod Impact, Notched 0.530 J/cm
@Temperature 23.0 °C
0.993 ft-lb/in
@Temperature 73.4 °F
Method A; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C190 °Funannealed; ASTM D648
 
Descriptive Properties
Processing MethodCompounding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Pro-fax 6301 Polypropylene Homopolymer, Flake Resin

PEQT8796 / 220430

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.