MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Morbond 170 Chamotte/Bauxite Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Chemical bond. Morbond 170 is a two component system that forms a rapid setting, easily placed castable on mixing, which can be brought quickly into service. Morbond 170 is a chamotte/bauxite composition exhibiting excellent thermal shock resistance. Specifically developed for heat containment applications, it is particularly recommended for burner quarls. For any non-metal contact application where severe thermal shock is encountered.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 2.50 g/ccdried to 110°C
Grain Size <= 4000 µm
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 30.0 MPa
@Treatment Temp. 110 °C
Cold Crushing Strength
 30.0 MPa
@Treatment Temp. 815 °C
Cold Crushing Strength
 30.0 MPa
@Treatment Temp. 1000 °C
Cold Crushing Strength
 65.0 MPa
@Treatment Temp. 1600 °C
Cold Crushing Strength
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air <= 1700 °C
Shrinkage -0.500 - 0.50 %
@Treatment Temp. 1600 °C
 0.10 %
@Treatment Temp. 815 °C
 0.10 %
@Treatment Temp. 1000 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 75 %
CaO 2.0 %
Fe2O3 0.60 %
K2O+Na2O 0.20 %Na2O+ K2O
MgO 0.10 %
P2O5 5.4 %
SiO2 15 %
TiO2 1.4 %
 
Descriptive Properties
Net Material Required (kg/m³)2450
Water AdditionAccelerator, 1 bottle, 25 kg bag weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF6238 / 203022

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.