MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Texmar 16 SG SAE 30
Categories: Fluid; Lubricant

Material Notes: Texaco Texmar 16 SG delivers value through:
  • Wear protection — Texaco Texmar 16 SG oil has superior anti-wear characteristics to reduce wear on all moving engine components. Controls ring and liner wear through its ability to neutralize acids formed by the combustion of sulfur in fuel, thereby permitting longer overhaul periods. Contains high performance antiwear additives, providing excellent protection for cams, camshaft and bearings.
  • Prevention of deposits and sludge — Prevents the formation of high temperature piston deposits, as well as low temperature sludge, in order to guarantee continuous oil flow inside the engine.
  • Oxidation stability — Provides a very high thermal and oxidation stability withstanding high thermal stresses of high output trunk piston engines and reducing undercrown deposits.
  • Rust protection — Effective inhibitor package prevents rusting in stern tube applications.

Texaco Texmar 16 SG oil is a high performance, medium alkaline diesel engine oil for medium and highspeed trunk piston diesel engines.

Texaco Texmar 16 SG oil, 16 base number oil, is blended from highly refined quality base oils in combination with a specially developed package containing alkaline detergents, dispersants, oxidation and corrosion inhibitors and anti-wear additives.

Texaco Texmar 16 SG oil is recommended for the lubrication of medium and high-speed turbo charged and naturally aspirated diesel engines, operating on gas oil and marine diesel oil containing low to medium sulfur levels (up to 1.8%).

Texaco Texmar 16 SG is especially developed for marine and power generation applications. Taro 16 SG oil is highly suitable for applications that include a separator in the lubrication system. Texaco Texmar 16 SG oil can be used in a multitude of applications such as reduction gears, air compressors, medium loaded gear applications, stern tubes, propulsion and auxiliary engines.

Texaco Texmar 16 SG oil meets the requirements of the major high and medium-speed marine diesel engine manufacturers.

Texaco Texmar 16 SG oil meets the performance requirements of API Service Category CF.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 220846; MSDS Number: 10270

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 28.4 °
Viscosity Measurement 97Viscosity Index
Kinematic Viscosity at 40°C (104°F) 93 cSt
Kinematic Viscosity at 100°C (212°F) 11 cSt
Ash 1.95 %Sulfated Ash, mass %
 
Chemical PropertiesOriginal ValueComments
Total Base Number 16ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -15.0 °C
Flash Point 240 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik CS-9A Precision Wire
316 Stainless Steel, spring tempered wire, 1.6 mm diam.
Alcoa 2090-T83 Aluminum
Beryllium I-220H Instrument Grade
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP

WTEXA202 / 77081

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.