MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

The NanoSteel® Company SHS 9570 TWAS Steel Alloy, Cored Wire  (discontinued **)
Categories: Metal; Ferrous Metal; Alloy Steel; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Coating Description: SHS 9570 TWAS is an iron based steel alloy with a nanoscale microstructure that features superior toughness with good combined wear, impact and corrosion resistance.

    Key Performance Characteristics
  • Excellent corrosion resistance while maintaining high impact and wear resistance
  • Superior toughness and resiliency
  • Alternative to nickel superalloys and stainless steels
  • Cost-effective option for rebuilding worn out components and parts

Application Process: Twin Wire Arc Spraying (TWAS)

Information Provided by The NanoSteel Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.59 g/cc0.274 lb/in³Coating Property
Porosity <= 5.0 %<= 5.0 %Coating Property
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 850 - 950850 - 950kg/mm2; HV300
Adhesive Bond Strength 34.5 - 48.3 MPa
@Thickness 0.508 mm
5000 - 7000 psi
@Thickness 0.0200 in
1018 steel; ASTM C633-01
 
Component Elements PropertiesMetricEnglishComments
Boron, B <= 10 %<= 10 %
Carbon, C <= 5.0 %<= 5.0 %
Chromium, Cr <= 25 %<= 25 %
Iron, Fe >= 23 %>= 23 %
Manganese, Mn <= 5.0 %<= 5.0 %
Niobium, Nb (Columbium, Cb) <= 20 %<= 20 %
Silicon, Si <= 2.0 %<= 2.0 %
Tungsten, W <= 10 %<= 10 %
 
Descriptive Properties
Deposition Efficiency (%)80Coating Property
Impact ResistanceNo delamination/cracking at 480 in-lbsDrop Impact Testing
Wear Resistance Mass Loss (g)0.252000 cycles; ASTM G65-04 Procedure B

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Universal Wire Works ER240 Stainless Steel Bare Wire
AISI 302Cu Stainless Steel soft tempered 2.54- 25.4 mm diameter wire
446 Stainless Steel, Soft Tempered Wire
430 Stainless Steel soft tempered wire 6.4 mm diameter
430 Stainless Steel annealed wire 6.4 mm diameter

NNANO104 / 106805

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.