C8904XXX is PVC compound product with any color for using in wire and cable application product. The formulation is designed for Insulation 70 ° C rated low end cable which give good process ability by extrusion. Applications: Insulation 70 ° C rated low end cable. Features: Good process ability. Good surface of product. Information provided by SCG. |