MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chemical Concepts Rodmaster 6600 Quick Set Methacrylate adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: ChemSet Rodmaster 6600 Quick Set is a high performance two part methacrylate adhesive engineered for rodding natural stone. It offers outstanding bond strength, is extremely durable, with excellent impact and weathering properties. Rodmaster 6600 greatly increases the durability of rodded stone, improving the stone's load capacity up to fives times compared to polyesters and other adhesives. It offers exceptional flexibility, the ability to withstand extreme temperature fluctuation and thermal cycling and resistance to a wide range of chemicals and environmental conditions. Rodmaster 6600 offers exceptional bonding capability to a wide range of substrates, including metals, plastics, composites and ceramics making it suitable for many other applications.

Quick Working Time: This adhesive has a working time of 4 minutes and reaches handing strength in 10 minutes. No need to wait for the stone to dry: No more blow torching or long waiting times. 5-10x the strength compared to polyesters. Exceptional Flexibility. Easy-to-Use Cartridge: No more hand mixing, always a consistent mixture.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.959 g/cc0.0346 lb/in³activator
 0.971 g/cc0.0351 lb/in³mixed
 0.983 g/cc0.0355 lb/in³resin
Viscosity 40000 - 90000 cP40000 - 90000 cPresin
 100000 - 150000 cP100000 - 150000 cPactivator
 60000 cP
@Temperature 25.0 °C
60000 cP
@Temperature 77.0 °F
resin, uncured
 60000 cP
@Temperature 25.0 °C
60000 cP
@Temperature 77.0 °F
activator, uncured
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 17.2 MPa>= 2500 psi
Shear Strength >= 17.2 MPa>= 2500 psicured
 
Thermal PropertiesMetricEnglishComments
Flash Point 10.6 °C51.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 18.3 - 29.4 °C65.0 - 85.0 °F
Working Life 3.00 - 6.00 min
@Temperature 23.0 °C
3.00 - 6.00 min
@Temperature 73.4 °F
 
Descriptive Properties
Coloramber, activator, uncured
 translucent, resin
Fixture Time10 to 15 minutes @ 75°F
Gap Filling0.25 inches
Mix Ratioresin 1.0: activator 1.0
Thix Index5
Time before moving18 to 24 minutes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHEMI984 / 232154

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.