MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ChevronTexaco 2190 T-EP Military Symbol Oil
Categories: Fluid; Lubricant

Material Notes: Texaco Military Symbol Oil 2190 T-EP delivers value through:
  • Long lubricant life because of selected base stocks and additives.
  • Extreme pressure characteristics that provide high film strength to protect gears and bearings engaged in severe, heavy-duty service.
  • MIL-L-17331H(SH) qualified — Meets stringent military specifications.
  • High viscosity index — Minimal viscosity change in broad operating temperature range enhances lubricant film strength.

Texaco Military Symbol Oil 2190 T-EP was developed primarily as a circulating system oil for marine gear turbine sets.

  • Texaco Military Symbol Oil 2190 T-EP provides mild extreme pressure protection as well as resistance to rust, oxidation, corrosion, and foaming.
  • Texaco Military Symbol Oil 2190 T-EP has outstanding thermal and oxidation stability that allows it to withstand the high temperatures found in turbine bearing and gear lubrication.
  • The foam inhibition prevents the buildup of foam in the sump tank with possible vent pipe overflow.
  • Its excellent stability, high viscosity index, and rust and corrosion inhibition assures high film strength lubrication for gears and bearings, as well as rust and corrosion protection. Together, these qualities mean both long lubricant and equipment life.

    Texaco Military Symbol Oil 2190 T-EP is recommended for use in marine turbine reduction gears, where heavy tooth loading and shock loads are encountered.

    The extreme pressure properties enable Texaco Military Symbol Oil 2190 T-EP to meet the requirements of MIL-L-17331H(SH) Amendment 3, Symbol 2190 TEP.

    Do not filter through Fullers Earth-type filtration systems since this would deplete the additive package.

    Do not use in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed.

    Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

    CPS Number: 221546; MSDS Number: 8695

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    API Gravity 31.9 °31.9 °
    Viscosity Measurement 9999Viscosity Index
    Saybolt Viscosity at 100°F 415 SUS415 SUS
    Saybolt Viscosity at 210°F 59.1 SUS59.1 SUS
    Kinematic Viscosity at 40°C (104°F) 79.8 cSt79.8 cSt
    Kinematic Viscosity at 100°C (212°F) 9.7 cSt9.7 cSt
    Ash <= 0.0010 %<= 0.0010 %Sulfated Ash
    ASTM Color 0.500.50ASTM D1500
     
    Chemical PropertiesMetricEnglishComments
    Acid Value 0.160.16mg KOH/g; ASTM D974
     
    Thermal PropertiesMetricEnglishComments
    Pour Point -12.0 °C10.4 °F
    Flash Point 246 °C475 °F
     
    Descriptive Properties
    Conradson Carbon Residue, mass%0.1
    Corrosion, Copper Strip13 h at 100°C
    Rust PreventionPass48 h, Oil water washed

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    WTEXA110 / 76989

    New MatWeb Services

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.