Soft, flexible polyurethane elastomer Key Properties: - Excellent physical properties after RT cure
- Free of mercury, MOCA or TDI
- Raw materials meet FDA code standards
Applications: - For hand-batch processing
- FDA CFR 177.1680
- FDA CFR 177.105
- FDA CFR 177.2600
Cure 1: 2 hour at 150°F + 7 days at 77°FInformation provided by © RAMPF Tooling Solutions GmbH & Co. KG |