MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
A286 IRON BASED 15Cr-26Ni-1.3Mo-2.1Ti-0.3V SUPERALLOY FORGINGS FOR GAS TURBINE DISCS
Categories: Metal; Ferrous Metal; Stainless Steel; Superalloy; Iron Base

Material Notes:

Creep and rupture data provided by NIMS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 304
Tensile Strength, Ultimate 1035 MPa
Tensile Strength, Yield 760 MPa
Elongation at Break 25 %
Rupture Strength 110 MPa
@Temperature 675 °C,
Time 3.60e+8 sec
 95.0 - 143 MPa
@Temperature 650 °C,
Time 3.60e+8 sec
 139 - 186 MPa
@Temperature 625 °C,
Time 3.60e+8 sec
 205 - 247 MPa
@Temperature 600 °C,
Time 3.60e+8 sec
 281 - 321 MPa
@Temperature 575 °C,
Time 3.60e+8 sec
 364 - 394 MPa
@Temperature 550 °C,
Time 3.60e+8 sec
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 13 - 17 %
Iron, Fe 53 - 55 %
Molybdenum, Mo 1.1 - 1.5 %
Nickel, Ni 24 - 28 %
Titanium, Ti 2.0 - 2.2 %
Vanadium, V 0.20 - 0.40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum Altemp® A286 Iron-Base Superalloy, UNS S66286
ATI Allvac® Nickelvac® A-286 Specialty Steel, Heat Treatment: 982°C (1800°F) + Age
660 Stainless Steel (A286) cold drawn wire diameter of 4.45 mm, aged at 540°C (1000°F)
660 Stainless Steel (A286) short time tensile test
Pyramid Stainless Steel AISI 304/316L, STAINLESS STEEL SHEET NO.4 FINISH

NIMS030 / 77547

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.