MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® M76/M46J Curing Epoxy Matrix with Fibers
Categories: Polymer; Thermoset; Epoxy

Material Notes:

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Outgassing - Total Mass Loss 0.000 %CVCM; ASTM E 595
 0.0700 %WVR; ASTM E 595
 0.130 %TML; ASTM E 595
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 58.0 MPa90°
 2172 MPa
Tensile Modulus 7.40 GPa90°
 273 GPa
Flexural Strength 1372 MPa
 993 MPa
@Temperature 121 °C
0°, Wet
Flexural Modulus 228 GPa
 239 GPa
@Temperature 121 °C
0°, Wet
Compressive Strength 1082 MPa
Compressive Modulus 239 MPa
Shear Strength 97.0 MPaShort Beam, 42 Day; ASTM 2344
 98.0 MPaInterlaminar, 0°
 100 MPaShort Beam, 56 Day; ASTM 2344
 101 MPaShort Beam, 14 Day; ASTM 2344
 101 MPaShort Beam, 21 Day; ASTM 2344
 101 MPaShort Beam, 7 Day; ASTM 2344
 102 MPaShort Beam, 28 Day; ASTM 2344
 103 MPaShort Beam, 1 Day; ASTM 2344
 61.0 MPa
@Temperature 121 °C
Interlaminar, 0°, Wet
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 157 °C56 Day; T41
 158 °C28 Day; T41
 158 °C42 Day; T41
 159 °C1 Day; T41
 159 °C14 Day; T41
 159 °C7 Day; T41
 160 °C21 Day; T41
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature -18.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHEXCB9148 / 322304

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.