MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
A. Schulman Diamond Centrex® 814 General Purpose Injection Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: Centrex 814 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and processing performance, along with good resistance to weather aging.

Applications: Typical applications for Centrex 814 resin includes exterior parts such as marine components, pool accessories, spa components, lawn and garden accessories, large, outdoor TV screen displays; pool accessories, recreation vehicle components and outdoor advertising sign parts. As with any product, use of Centrex 814 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Weatherable Polymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0060 cm/cmASTM D955
Melt Flow 9.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 101ASTM D785
Tensile Strength, Yield 38.5 MPachs 2.0 in/min; ASTM D638
Tensile Modulus 2100 MPachs 2.0 in/min; ASTM D638
Flexural Strength 68.7 MPachs 0.05 in/min; ASTM D790
Flexural Modulus 2200 MPatangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 75.0 J/m
@Thickness 3.17 mm,
Temperature -30.0 °C
ASTM D256
 270 J/m
@Thickness 3.17 mm,
Temperature 23.0 °C
ASTM D256
Impact Test 8.20 J
@Temperature -30.0 °C
ASTM D3763
 33.0 J
@Temperature 23.0 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C0.125";; ASTM D648
 77.0 °C0.25";; ASTM D648
Vicat Softening Point 101 °C
@Load 1.00 kg
120°C/hr; ASTM D1525
Flammability, UL94 HB
@Thickness 0.749 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Lustran® 256/Lustran® 752 Blended ABS Resin
A. Schulman Diamond ASA S210B
A. Schulman Diamond ASA TW18B3 ASA Weatherable Polymers Injection Molding Grade, Very High Heat
A. Schulman Diamond Centrex® 810 Injection Molding Grade
A. Schulman Diamond Centrex® 821 ASA Weatherable Polymers Injection Molding Grade

PDIAM354 / 126445

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.