MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

CLAL-MSX NICLAL 3444 0 Annealed Copper Alloy, Free Cutting Bronze
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Main Characteristics:
  • Excellent machineability
  • High mechanical properties
  • Self lubricating alloy
Typical Applications:
  • Parts for connectors
  • Friction parts
  • Bearings-Pinions-Lock pins

Information provided by CLAL-MSX

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.90 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers <= 90<= 90
Tensile Strength, Ultimate <= 400 MPa<= 58000 psi
Tensile Strength, Yield >= 100 MPa
@Strain 0.2 %
>= 14500 psi
@Strain 0.2 %
Elongation at Break >= 35 %>= 35 %100 A
Modulus of Elasticity 105 GPa15200 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000101 ohm-cm0.0000101 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.3 µm/m-°C
@Temperature 0.000 - 100 °C
9.61 µin/in-°F
@Temperature 32.0 - 212 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 67.0 W/m-K465 BTU-in/hr-ft²-°F
Melting Point 930 °C1710 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 88 %88 %
Lead, Pb <= 4.0 %<= 4.0 %
Tin, Sn 4.0 %4.0 %
Zinc, Zn <= 4.0 %<= 4.0 %
 
Descriptive Properties
ColorBronze

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CLAL-MSX NICLAL 1300 0 Annealed Copper Alloy, Free Cutting Nickel-Silver
CLAL-MSX NICLAL 1800 0 Annealed Copper Alloy, Free Cutting Nickel-Silver
Cartridge Brass, UNS C26000 (260 Brass), H08 Temper flat products
Copper, Cu; Annealed
Overview of materials for Copper Alloy

NCLAL089 / 160120

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.