MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ArcelorMittal FB 450 Hot rolled ferrite-bainite steel
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Available in the following: uncoated (HDT450F) and Extragal® (HDT450F+Z)

Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It comprises four strength levels: FB 450, 540, 560 and 590. This family of steels extends the HSLA range of micro-alloyed steels to include products combining high tensile strength (UTS) with excellent formability and hole expansion (stretch flangeability) based on their ferrite-bainite microstructure.

Applications: These steels are cold-drawn. The main applications are:

  • structural parts (longitudinal beams, cross beams, car-body and ground liason parts),
  • wheels,
  • mechanical parts (ground liason parts, gear boxes...).
ArcelorMittal has an extensive database relating to the forming and service properties of the entire range of ferrite-bainite steels. To integrate these steels at the design stage, a team of experts is available to perform specific studies based on modeling or laboratory tests.

Information provided by ArcelorMittal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 450 - 510 MPa65300 - 74000 psi
Tensile Strength, Yield 300 - 380 MPa43500 - 55100 psi
Elongation at Break >= 25 %>= 25 %L0=80 mm, th<3 mm
 >= 32 %>= 32 %L0=5.65v 0 mm, th<3 mm
Fatigue Strength  <= 320 MPa
@# of Cycles 2.00e+6
<= 46400 psi
@# of Cycles 2.00e+6
 <= 320 MPa
@# of Cycles 1.00e+7
<= 46400 psi
@# of Cycles 1.00e+7
 <= 400 MPa
@# of Cycles 100000
<= 58000 psi
@# of Cycles 100000
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.17 %<= 0.17 %
Iron, Fe >= 98.98 %>= 98.98 %as balance
Manganese, Mn <= 0.80 %<= 0.80 %
Silicon, Si <= 0.050 %<= 0.050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ArcelorMittal FB 560 Hot rolled ferrite-bainite steel
AISI 1108 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Envalior Novamid® 1013GH45 1 NA/BK701 PA6-GF45
AISI 1020 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 25 mm (1 in.) round
AISI 1019 Steel, cold drawn

NARCE033 / 159941

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.