Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.18 g/cc | 1.18 g/cc |
Density | 1.19 g/cc | 0.0430 lb/in³ |
Moisture Absorption | 0.150 % @Temperature 23.0 °C | 0.150 % @Temperature 73.4 °F |
Water Absorption at Saturation | 0.35 % @Temperature 23.0 °C | 0.35 % @Temperature 73.4 °F |
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm | 0.0040 - 0.0080 in/in @Thickness 0.126 in |
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm | 0.0040 - 0.0080 in/in @Thickness 0.126 in |
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C | 9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
| 10 g/10 min @Load 1.20 kg, Temperature 300 °C | 10 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, H358/30 | 90.0 MPa | 13100 psi |
Tensile Strength at Break | 60.0 MPa | 8700 psi |
| 61.0 MPa | 8850 psi |
Tensile Strength, Yield | 55.0 MPa | 7980 psi |
| 58.0 MPa | 8410 psi |
Elongation at Break | 125 % | 125 % |
| 130 % | 130 % |
Elongation at Yield | 6.0 % | 6.0 % |
| 6.0 % | 6.0 % |
Tensile Modulus | 2.10 GPa | 305 ksi |
| 2.10 GPa | 305 ksi |
Flexural Yield Strength | 85.0 MPa | 12300 psi |
| 88.0 MPa | 12800 psi |
Flexural Modulus | 2.06 GPa | 299 ksi |
| 2.20 GPa | 319 ksi |
Izod Impact, Notched | 10.68 J/cm | 20.01 ft-lb/in |
| 5.87 J/cm @Temperature -50.0 °C | 11.0 ft-lb/in @Temperature -58.0 °F |
| 6.78 J/cm @Temperature -30.0 °C | 12.7 ft-lb/in @Temperature -22.0 °F |
| 8.01 J/cm @Temperature 23.0 °C | 15.0 ft-lb/in @Temperature 73.4 °F |
| 6.40 J/cm @Thickness 6.40 mm, Temperature 23.0 °C | 12.0 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C | 26.2 ft-lb/in² @Temperature -22.0 °F |
| 65.0 kJ/m² @Temperature -30.0 °C | 30.9 ft-lb/in² @Temperature -22.0 °F |
| 70.0 kJ/m² @Temperature 23.0 °C | 33.3 ft-lb/in² @Temperature 73.4 °F |
| 80.0 kJ/m² @Temperature 23.0 °C | 38.1 ft-lb/in² @Temperature 73.4 °F |
Izod Impact, Unnotched (ISO) | NB @Temperature -30.0 °C | NB @Temperature -22.0 °F |
| NB @Temperature 23.0 °C | NB @Temperature 73.4 °F |
Charpy Impact Unnotched | NB @Temperature -30.0 °C | NB @Temperature -22.0 °F |
| NB @Temperature 23.0 °C | NB @Temperature 73.4 °F |
Charpy Impact, Notched | 6.00 J/cm² @Temperature -30.0 °C | 28.6 ft-lb/in² @Temperature -22.0 °F |
| 7.50 J/cm² @Temperature 23.0 °C | 35.7 ft-lb/in² @Temperature 73.4 °F |
Instrumented Impact Total Energy | 52.0 J @Temperature 23.0 °C | 38.4 ft-lb @Temperature 73.4 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm |
Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm |
Dielectric Constant | 2.6 @Frequency 50.0 - 60.0 Hz | 2.6 @Frequency 50.0 - 60.0 Hz |
| 2.7 @Frequency 1e+6 Hz | 2.7 @Frequency 1e+6 Hz |
| 2.9 @Frequency 1e+6 Hz | 2.9 @Frequency 1e+6 Hz |
| 2.95 @Frequency 50.0 - 60.0 Hz | 2.95 @Frequency 50.0 - 60.0 Hz |
Dielectric Strength | 16.0 kV/mm @Thickness 3.20 mm | 406 kV/in @Thickness 0.126 in |
| 17.0 kV/mm @Thickness 3.20 mm | 432 kV/in @Thickness 0.126 in |
Dissipation Factor | 0.0010 @Frequency 50.0 - 60.0 Hz | 0.0010 @Frequency 50.0 - 60.0 Hz |
| 0.0024 @Frequency 50.0 - 60.0 Hz | 0.0024 @Frequency 50.0 - 60.0 Hz |
| 0.0085 @Frequency 1e+6 Hz | 0.0085 @Frequency 1e+6 Hz |
| 0.0085 @Frequency 1e+6 Hz | 0.0085 @Frequency 1e+6 Hz |
Comparative Tracking Index | 175 - 250 V | 175 - 250 V |
| 225 V | 225 V |
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec |
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear, Parallel to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C | 37.0 µin/in-°F @Temperature -40.0 - 104 °F |
| 72.0 µm/m-°C @Temperature 23.0 - 80.0 °C | 40.0 µin/in-°F @Temperature 73.4 - 176 °F |
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C | 37.0 µin/in-°F @Temperature -40.0 - 104 °F |
| 77.0 µm/m-°C @Temperature 23.0 - 80.0 °C | 42.8 µin/in-°F @Temperature 73.4 - 176 °F |
Hot Ball Pressure Test | 125 °C | 257 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 135 °C | 275 °F |
| 134 °C @Thickness 3.20 mm | 273 °F @Thickness 0.126 in |
Deflection Temperature at 1.8 MPa (264 psi) | 124 °C | 255 °F |
| 120 °C @Thickness 3.20 mm | 248 °F @Thickness 0.126 in |
| 124 °C @Thickness 6.40 mm | 255 °F @Thickness 0.252 in |
Vicat Softening Point | 140 °C | 284 °F |
| 142 °C | 288 °F |
| 142 °C | 288 °F |
UL RTI, Electrical | 125 °C | 257 °F |
UL RTI, Mechanical with Impact | 115 °C | 239 °F |
UL RTI, Mechanical without Impact | 120 °C | 248 °F |
Flammability, UL94 | V-0 @Thickness 1.49 mm | V-0 @Thickness 0.0587 in |
| 5VA @Thickness 2.99 mm | 5VA @Thickness 0.118 in |
Oxygen Index | 35 % | 35 % |
Glow Wire Ignition Temperature | 825 °C @Thickness 1.00 mm | 1520 °F @Thickness 0.0394 in |
Glow Wire Flammability Index | 960 °C @Thickness 1.00 mm | 1760 °F @Thickness 0.0394 in |
|
Descriptive Properties |
---|
UV-light, water exposure/immersion | F1 |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.