MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Chevron Phillips K-Resin® CK02 Styrene-Butadiene Copolymer, Blow Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styrene-Butadiene Copolymer

Customer Benefits: CK02 is a blow molding SBC designed to provide a softer, tougher, more flexible container while retaining the clarity and gloss of bottles produced from KR05. Finished products have low stiffness, excellent clarity, high surface gloss, and excellent toughness. K-Resin provides integral handles and wide mouth containers.

Applications: Major applications include squeeze bottles, food containers, medical packaging, and toys.

Processing Recommendations:
Can be processed on extrusion blow, injection stretch, and injection blow. Extrusion: Recommended maximum melt temperature is 195°C. Injection: Recommended maximum melt temperature, 216°C. High shear and restrictive type screws tend to degrade the melt. Generally no need to dry resin.

Specification Data: FDA Regulation 21 CFR 177.1640; suitable for food contact. EEC Directive 90/128/EEC and all its amendments. USP Class VI-50.

Data provided by Chevron Phillips Chemical Company LP.

Ineos Styrolution acquired the K-Resin® product line from Chevron Phillips Chemical Company in 2016. This grade was previously discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 91ASTM D2240
Tensile Strength, Yield 15.2 MPa2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Elongation at Break 330 %2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Flexural Yield Strength 22.2 MPaTest specimens were injection molded by ASTM D1897; ASTM D790
Flexural Modulus 0.696 GPaTest specimens were injection molded by ASTM D1897; ASTM D790
Izod Impact, Notched NBASTM D256
Instrumented Impact Total Energy 37.6 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 39.0 °CASTM D648
Vicat Softening Point 59.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Gloss 146 %60°
Transmission, Visible 91 %
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 216 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
USP Class VI Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips K-Resin® KR10 Styrene-Butadiene Copolymer, Film Grade
Chevron Phillips K-Resin® KR99HG Styrene-Butadiene Copolymer, Injection Molding Grade
Chevron Phillips K-Resin® BK11 Styrene-Butadiene Copolymer, Injection Molding Grade
Chevron Phillips K-Resin® BK15 Styrene-Butadiene Copolymer, Injection Molding Grade
Chevron Phillips K-Resin® XK40 Styrene-Butadiene Copolymer, Sheet Grade

PCHEVK25 / 20278

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.