MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Novec™ 1710 Electronic Grade Coating
Categories: Polymer

Material Notes: 3M™ Novec™ 1710 Electronic Grade Coating is a higher solids version of Novec™ 1700. It is a clear, low viscosity, low surface tension solution of a 10 wt% fluorochemical acrylic polymer carried in a hydrofluoroether solvent.

Features and Benefits:

  • Can be used as a concentrate for maintaining coating solids concentration in application baths or incorporated with resins or other liquids for a unique solution.
  • Easy application and processing – dries in seconds without the need for thermal post-curing
  • Contains no volatile organic compounds (VOCs) and has low global warming potential
  • Provides excellent repellency, anti-wetting and anti-sticking properties against liquids, water, hydrocarbons, silicones, and photoresists

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³
Solids Content 10 %10 %fluoropolymer
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.1
@Frequency 1000 Hz
3.1
@Frequency 1000 Hz
30% RH
Dielectric Strength 3.94 kV/mm100 kV/in35% RH
Dissipation Factor 0.0089
@Frequency 1000 Hz
0.0089
@Frequency 1000 Hz
30% RH
 
Thermal PropertiesMetricEnglishComments
Boiling Point 61.0 °C142 °Fof Solvent
Glass Transition Temp, Tg 44.5 °C112 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.391.39
 
Processing PropertiesMetricEnglishComments
Shelf Life 48.0 Month48.0 Monthfrom date of manufacture in unopened container

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shandong Dongyue Polymer DF-21 PTFE Presintered Resin

PMM33098 / 167845

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.