MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Cabot ELFTEX® S5100 Specialty Carbon Black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product highlights: ELFTEX S5100 specialty carbon black is a high structure carbon black suitable for use in a variety of adhesives, sealants plastics, inks and coatings applications. This product is in powder form for easier dispersion in low shear process equipment.

Key applications:
Rheology and reinforcement of structural adhesives and sealants: ELFTEX S5100 specialty carbon black is suitable for use in structural adhesives for transportation manufacturing applications, such as windshield bonding, and construction adhesives and sealants.
Pigmentation in plastics, inks and coatings: ELFTEX S5100 specialty carbon black can also be used for pigmentation in a variety of plastics, inks and coatings applications including industrial, decorative and powder coatings. It also is suitable for use in the coloration of dispersions for leather.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Mesh Size 325 Mesh325 Mesh<250 ppm residue; ASTM D-1514
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 1.0 %<= 1.0 %ASTM D-1509
 
Descriptive Properties
Iodine absorption91 mg/gASTM D-1510
OAN108 cc/100gASTM D-2414

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT125 / 315860

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.