Key features of this grade: High moisture and chemical resistance. Good adhesion. Excellent thermal properties. VOC-free. Vacuum pressure impregnation (VPI) is mainly used when the penetration and filling factor of the resin need to be improved versus other processing options. Information provided by Von Roll. |