MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Domo TECHNYL® A 258 PA Black 2N PA66, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Description: Unreinforced and modified polyamide 66, UV and thermal stabilized with excellent impact resistance, for injection molding.

Available in: Europe

Product Applications: TECHNYL® A 258P1 BLACK 2N offers excellent impact resistance properties at ambient and low temperature and special low rigidity. This grade is commonly used for fasteners, cable ties and dowels. This product is available in black.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 44.0 MPa6380 psiISO 527 Type 1A
Elongation at Break 290 %290 %ISO 527 Type 1A
Tensile Modulus 1.175 GPa170.4 ksiISO 527 Type 1A
Charpy Impact, Notched  1.17 J/cm²
@Temperature -30.0 °C
5.57 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 9.05 J/cm²
@Temperature 23.0 °C
43.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
1210
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
1210
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
1210
 
Processing PropertiesMetricEnglishComments
Feed Temperature 260 - 270 °C500 - 518 °F
Mold Temperature 50.0 °C122 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone270-275°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRHOD701 / 137932

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.