MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Parker Chomerics CHO-MUTE 9000 Microwave Absorber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicone polymer system that offers the benefit of wide band absorption and high permeability in a lightweight and flexible product form.

Applications:

    CHO-MUTE 9000 is effective in many applications to eliminate EMI/EMC problems in, transmitters, transceivers, microcontrollers, microprocessors etc.
  • Hand held electronics, wireless voice or data telecommunications, infotainment, testing equipment, PDAs
  • Military electronics C3l, navigation, GPS, ruggedized computers, night vision
  • Antenna performance, surface current reduction
  • Office and telecommunication infrastructure equipment, computing, switch gear, power amplifiers, routers

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.40 g/cc3.40 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5555
Tensile Strength at Break 3.45 MPa500 psi
Elongation at Break >= 200 %>= 200 %
Tear Strength 10.5 kN/m59.9 pli
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+6 ohm-cm>= 1.00e+6 ohm-cm
Surface Resistivity per Square >= 1.00e+6 ohm>= 1.00e+6 ohm
Shielding Effectiveness  -23.0 dB
@Thickness 1.57 mm,
Frequency 8.00e+9 Hz
-23.0 dB
@Thickness 0.0620 in,
Frequency 8.00e+9 Hz
Microwave Absorption
 -21.0 dB
@Thickness 2.36 mm,
Frequency 6.00e+9 Hz
-21.0 dB
@Thickness 0.0930 in,
Frequency 6.00e+9 Hz
Microwave Absorption
 -14.0 dB
@Thickness 1.57 mm,
Frequency 1.05e+10 Hz
-14.0 dB
@Thickness 0.0620 in,
Frequency 1.05e+10 Hz
Microwave Absorption
 -13.0 dB
@Thickness 0.813 mm,
Frequency 1.05e+10 Hz
-13.0 dB
@Thickness 0.0320 in,
Frequency 1.05e+10 Hz
Microwave Absorption
 -12.0 dB
@Thickness 3.17 mm,
Frequency 4.00e+9 Hz
-12.0 dB
@Thickness 0.125 in,
Frequency 4.00e+9 Hz
Microwave Absorption
 -10.0 dB
@Thickness 1.57 mm,
Frequency 1.55e+10 Hz
-10.0 dB
@Thickness 0.0620 in,
Frequency 1.55e+10 Hz
Microwave Absorption
 -7.00 dB
@Thickness 2.36 mm,
Frequency 1.05e+10 Hz
-7.00 dB
@Thickness 0.0930 in,
Frequency 1.05e+10 Hz
Microwave Absorption
 -7.00 dB
@Thickness 0.813 mm,
Frequency 1.55e+10 Hz
-7.00 dB
@Thickness 0.0320 in,
Frequency 1.55e+10 Hz
Microwave Absorption
 -7.00 dB
@Thickness 1.57 mm,
Frequency 5.00e+9 Hz
-7.00 dB
@Thickness 0.0620 in,
Frequency 5.00e+9 Hz
Microwave Absorption
 -7.00 dB
@Thickness 1.57 mm,
Frequency 5.50e+9 Hz
-7.00 dB
@Thickness 0.0620 in,
Frequency 5.50e+9 Hz
Microwave Absorption
 -7.00 dB
@Thickness 2.36 mm,
Frequency 1.55e+10 Hz
-7.00 dB
@Thickness 0.0930 in,
Frequency 1.55e+10 Hz
Microwave Absorption
 -6.00 dB
@Thickness 3.17 mm,
Frequency 1.55e+10 Hz
-6.00 dB
@Thickness 0.125 in,
Frequency 1.55e+10 Hz
Microwave Absorption
 -5.00 dB
@Thickness 3.17 mm,
Frequency 5.50e+9 Hz
-5.00 dB
@Thickness 0.125 in,
Frequency 5.50e+9 Hz
Microwave Absorption
 -5.00 dB
@Thickness 3.17 mm,
Frequency 1.05e+10 Hz
-5.00 dB
@Thickness 0.125 in,
Frequency 1.05e+10 Hz
Microwave Absorption
 -5.00 dB
@Thickness 0.508 mm,
Frequency 1.05e+10 Hz
-5.00 dB
@Thickness 0.0200 in,
Frequency 1.05e+10 Hz
Microwave Absorption
 -4.00 dB
@Thickness 0.508 mm,
Frequency 1.55e+10 Hz
-4.00 dB
@Thickness 0.0200 in,
Frequency 1.55e+10 Hz
Microwave Absorption
 -3.00 dB
@Thickness 0.254 mm,
Frequency 1.55e+10 Hz
-3.00 dB
@Thickness 0.0100 in,
Frequency 1.55e+10 Hz
Microwave Absorption
 -3.00 dB
@Thickness 0.508 mm,
Frequency 5.50e+9 Hz
-3.00 dB
@Thickness 0.0200 in,
Frequency 5.50e+9 Hz
Microwave Absorption
 -3.00 dB
@Thickness 0.813 mm,
Frequency 5.50e+9 Hz
-3.00 dB
@Thickness 0.0320 in,
Frequency 5.50e+9 Hz
Microwave Absorption
 -3.00 dB
@Thickness 2.36 mm,
Frequency 2.50e+9 Hz
-3.00 dB
@Thickness 0.0930 in,
Frequency 2.50e+9 Hz
Microwave Absorption
 -3.00 dB
@Thickness 1.57 mm,
Frequency 2.50e+9 Hz
-3.00 dB
@Thickness 0.0620 in,
Frequency 2.50e+9 Hz
Microwave Absorption
 -2.00 dB
@Thickness 0.254 mm,
Frequency 1.05e+10 Hz
-2.00 dB
@Thickness 0.0100 in,
Frequency 1.05e+10 Hz
Microwave Absorption
 -1.00 dB
@Thickness 0.254 mm,
Frequency 5.50e+9 Hz
-1.00 dB
@Thickness 0.0100 in,
Frequency 5.50e+9 Hz
Microwave Absorption
 0.00 dB
@Thickness 0.254 mm,
Frequency 5.00e+8 Hz
0.00 dB
@Thickness 0.0100 in,
Frequency 5.00e+8 Hz
Microwave Absorption
 0.00 dB
@Thickness 0.508 mm,
Frequency 5.00e+8 Hz
0.00 dB
@Thickness 0.0200 in,
Frequency 5.00e+8 Hz
Microwave Absorption
 0.00 dB
@Thickness 0.813 mm,
Frequency 5.00e+8 Hz
0.00 dB
@Thickness 0.0320 in,
Frequency 5.00e+8 Hz
Microwave Absorption
 0.00 dB
@Thickness 1.57 mm,
Frequency 5.00e+8 Hz
0.00 dB
@Thickness 0.0620 in,
Frequency 5.00e+8 Hz
Microwave Absorption
 0.00 dB
@Thickness 2.36 mm,
Frequency 5.00e+8 Hz
0.00 dB
@Thickness 0.0930 in,
Frequency 5.00e+8 Hz
Microwave Absorption
 0.00 dB
@Thickness 3.17 mm,
Frequency 5.00e+8 Hz
0.00 dB
@Thickness 0.125 in,
Frequency 5.00e+8 Hz
Microwave Absorption
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.560 W/m-K3.89 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 160 °C320 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Descriptive Properties
CompositionFerrous filled silicone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics CHO-MUTE 9005 Microwave Absorber
Parker Chomerics CHO-MUTE 9020 RF Absorber
Hong Kun Group UV 123 UV Absorber
Parker Chomerics CHO-BOND® 1073, Part B Conductive Powder
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced

PCHOME096 / 28318

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.