MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Polytek TekBoard™ MB-5000 Polyurethane Board
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: TekBoard™ Tooling & Modeling Boards are pre-fabricated, highly machinable, dimensionally stable block materials that assist engineers, model makers, mechanical designers, and prototype developers in meeting the demanding needs of the aerospace, automotive, modeling, and prototyping industries. The Polytek® portfolio includes varying densities of urethane, aluminum-filled urethane and epoxy board materials.

TekBoard™ MB-5000 is a high-wear, white colored urethane board approximately with a ~100 lb/ft³ density. MB- 5000 is a high wear, high impact, urethane board that can be used for metal forming as well as nickel plating mandrels.

Information provided by Polytek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0579 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 86 - 9086 - 90
Tensile Strength 52.78 MPa7655 psi
Flexural Strength 68.8 MPa9980 psi
Flexural Modulus 4.72 GPa685 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 41.2 µm/m-°C22.9 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 90.6 °C195 °F
Glass Transition Temp, Tg 102 °C215 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTK5101 / 251093

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.