MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
PolyMirae Moplen EP336J Injection Molding Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Moplen EP336J is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP336J is a block copolymer selected by customers for use in injection molding of Toy, Crates. Moplen EP336J resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact.

Product Features: Optimized balance of stiffness and toughness/High impact strength at low temperature/High Stiffness/Low warpage

Typical Applications: Toy/Crate/Houseware

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASMT D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 86ASTM D785
Tensile Strength, Yield 250 kg(f)/cm²ASTM D638
Elongation at Yield 7.0 %ASTM D638
Flexural Modulus 12000 kg(f)/cm²ASTM D790
Izod Impact, Notched 6.00 kg-cm/cm
@Temperature -20.0 °C
ASTM D256
 45.0 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °CASTM D648
Vicat Softening Point 147 °CASTM D1525
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PolyMirae Moplen RP343N Injection Molding Grade Polypropylene
PolyMirae Clyrell EC340R Injection Molding Grade Polypropylene
PolyMirae Clyrell EC340Q Injection Molding Grade Polypropylene
PolyMirae Moplen RP340N Injection Molding Grade Polypropylene
PolyMirae Moplen HP640R Injection Molding Grade Polypropylene

PMIRAF14 / 183235

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.