MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Malleable Iron
Categories: Metal; Ferrous Metal; Cast Iron; Malleable Iron

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Malleable Iron". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 149 - 321Average value: 208 Grade Count:17
Hardness, Knoop 173 - 329Average value: 231 Grade Count:17
Hardness, Rockwell C 12.2 - 27.9Average value: 19.1 Grade Count:9
Hardness, Vickers 161 - 313Average value: 218 Grade Count:17
Tensile Strength, Ultimate 276 - 724 MPaAverage value: 498 MPa Grade Count:17
Tensile Strength, Yield 207 - 621 MPaAverage value: 371 MPa Grade Count:17
Elongation at Break 1.00 - 18.0 %Average value: 5.65 % Grade Count:17
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 2.00 - 2.70 %Average value: 2.41 % Grade Count:17
Chromium, Cr 0.0400 - 0.0700 %Average value: 0.0550 % Grade Count:7
Copper, Cu 0.0300 - 0.400 %Average value: 0.215 % Grade Count:7
Iron, Fe 94.4 - 96.0 %Average value: 95.1 % Grade Count:17
Manganese, Mn 0.250 - 1.25 %Average value: 0.585 % Grade Count:17
Molybdenum, Mo 0.0300 - 0.100 %Average value: 0.0650 % Grade Count:7
Nickel, Ni 0.0500 - 0.300 %Average value: 0.175 % Grade Count:7
Phosphorus, P 0.0300 - 0.0500 %Average value: 0.0418 % Grade Count:17
Silicon, Si 1.00 - 1.75 %Average value: 1.39 % Grade Count:17
Sulfur, S 0.0300 - 0.180 %Average value: 0.0865 % Grade Count:17

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Low Carbon Steel
Malleable iron casting, Class 32510
Overview of materials for Ductile Iron
Overview of materials for Medium Carbon Steel
Gray Cast Iron, ASTM A 48 Class 40

M01018 / 81725

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.