MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SunChemical Gwent C2100318D2 Silver Zinc Paste
Categories: Fluid; Metal; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: This product has been designed as a ‘one part system’ alternative to the traditional two part system. It is a screen printing ink for coating barium titanate PTC ceramic substrates.
Screen Printing Equipment: semi-automatic, manual
Screen Types: stainless steel, polyester, mesh 156-325 tpi
Substrate: Barium Titanate PTC ceramic parts

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 14750 - 16250 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
Haake VT 550 PK1.1°
Storage Temperature 20.0 °Csealed container
 
Processing PropertiesOriginal ValueComments
Sintering Temperature 560 - 630 °C
Cure Time 15.0 min
@Temperature 150 °C
Shelf Life 6.00 Month
 
Component Elements PropertiesOriginal ValueComments
Silver, Ag 58 %theoretical
Zinc, Zn 5.0 %theoretical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Elements Barium Titanate nanoparticles
Barium Titanate, BaTiO3
Harris Acoustic Sensors EC-21 Barium Titanate Piezoelectric
Channel Industries 300 Barium Titanate Piezoelectric
Channel Industries 1300 Barium Titanate Piezoelectric

WGELZ9070 / 139383

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.