MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eastman Llumar N1035B SR CDF (Bronze) Window Film
Categories: Polymer; Film

Material Notes: Neutral films reduce glare, provide moderate heat rejection, and are specified where a soft, neutral appearance is desired. These films are made with sputtered technology, creating a film that allows for very uniform visible light transmission. Neutral films are scratch-resistant and shield 99% of ultraviolet rays.

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 37 %37 %
UV Transmittance 26 %26 %Solar
Reflection Coefficient, Visible (0-1) 0.230.23Visible Reflectance (interior)
 0.260.26Visible Reflectance (exterior)
 0.370.37Total Solar Reflectance
 
Descriptive Properties
% Glare Reduction59
% Summer Solar Heat Gain Reduction58
% Total Solar Energy Rejected64
% Ultraviolet Ray Protection (wavelengths 300-380nm)99
% Winter Heat Loss Reduction12
Emissivity0.61
Light to solar gain (LSG)1.03
Shading coefficient0.41
Solar absorption37
Solar Heat Gain Coefficient0.36
U-value0.92Winter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5430 / 222624

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.